Common Mistakes in Carbon Brush Selection and Installation: Causes, Consequences, and Diagnostics

When original parts are unavailable and diagnostic equipment is limited, it is especially important to eliminate improper operation, perform scheduled maintenance, and follow the equipment manufacturer’s operating instructions.

This article reviews common mistakes in the selection and installation of carbon brushes. The recommendations below can help extend the service life of brush assemblies used in DC motors, conductor rail systems, and rotating electrical equipment.

1. What Are Carbon Brushes and What Are They Used For?

Carbon brushes are essential current-carrying components of a brush assembly. They provide electrical contact between the stationary and rotating parts of an electrical machine.

Carbon brushes are installed in brush holders—stationary assemblies equipped with springs that press the brush against the commutator or slip ring.

The brush is connected to the electrical circuit through a flexible conductor embedded in the brush body or through a spring-type connection attached to the brush.

The reliability and service life of electrical equipment with brush-type current collection depend directly on correct brush selection and installation.

A brush with the wrong material grade, dimensions, or design can cause serious equipment damage, including motor failure or emergency shutdown of a conductor rail system.

Carbon brushes are manufactured from electrographite materials, including grades with different percentages of metallic components. More than a thousand combinations of dimensions and designs are available.

2. Electrographite and Why It Is Used in Carbon Brushes

Electrographite is an engineered carbon material with stable electrical conductivity, high heat resistance, wear resistance, and controlled porosity. These properties are produced through a defined manufacturing process and are specified by material grade.

An electrographite grade is an alphanumeric designation that identifies key properties such as strength, electrical conductivity, density, ash content, and intended application.

“EG” grades — electrographite.
These grades contain no metallic additives.

  • Key characteristics: lower electrical conductivity than copper-graphite grades, high mechanical strength, good overload resistance, chemical stability, and resistance to high temperatures.

  • Applications: brushes for electric motors and generators.

“MG” grades — copper-graphite.
Copper alloy content ranges from approximately 15% to 95%.

  • Key characteristics: higher electrical conductivity than electrographite brushes, susceptibility to corrosion, and physical and technical properties that vary with temperature.

  • Applications: low-voltage electrical machines, starters, and generators.

Because of its layered crystal structure, graphite also performs an important lubricating function in sliding electrical contacts. It reduces the coefficient of friction and provides a self-lubricating effect. As a result:

  • wear of both contact surfaces is reduced;

  • a protective film, or patina, forms on the commutator surface, improving electrical contact and stabilizing operation;

  • the patina helps prevent scoring and overheating and acts as a thermally stable lubricant even at elevated temperatures;

  • contact becomes smoother and sparking is reduced under vibration and small mechanical fluctuations.

A properly engineered ratio of graphite and metallic, primarily copper, components makes it possible to produce brush materials whose physical and technical characteristics match the requirements of specific types of electrical machines. Correct material selection helps reduce losses and improve equipment efficiency.

Electrographite materials manufactured by qualified Russian producers can provide high performance and, depending on the grade, may be comparable with imported materials in their chemical and technical characteristics.

3. The Main Criterion for Carbon Brush Selection

There is only one basic principle: carbon brushes must be selected according to the physical and technical characteristics of the equipment in which they will operate.

This applies to electric motors, generators, conductor rail systems, and other rotating electrical equipment.

The required technical information is normally available either on the equipment nameplate or in the technical documentation and equipment data sheet.

Signs of an Incorrectly Selected Carbon Brush​​​​​​​

No.

Symptom / Indicator

Possible Causes

1

Excessive brush wear

Brush material is too soft, excessive current density, overheating.

2

Excessive sparking at the commutator or slip rings

Incorrect electrical conductivity, hardness, or material composition; poor brush seating.

3

Rapid commutator / slip-ring wear

Brush material is too hard or contains abrasive particles.

4

Unstable brush voltage, current fluctuations

Poor electrical contact; mismatch between the contact surface and brush material.

5

Uneven wear across the brush surface

Commutator deformation or out-of-round condition, poor brush seating, vibration, off-center installation, or incorrect brush dimensions.

6

Brush tilts or comes out of the brush holder

Brush material is too soft, excessive spring pressure, vibration, or worn brush-holder guides.

7

Brush assembly overheating

Excessive contact resistance, unsuitable electrographite composition, or sparking.

8

Dark deposits or excessive dust on the commutator

Breakdown of the binder material or unsuitable graphite structure.

9

Chipped or damaged brush edges

Brush material is too brittle or unsuitable for the operating vibration or temperature conditions.

10

Insufficient or uneven brush seating

Brush material is unsuitable for the operating speed, current load, or condition of the commutator.

4. Consequences of Incorrect Carbon Brush Selection

No.

Consequence

Description / Effect

Main Causes

1

Rapid brush wear and increased operating costs

Frequent replacement may be required. Chipping, breakage, or complete brush failure may occur.

Brush material is too soft, excessive current density, overheating, poor seating.

2

Commutator / slip-ring wear or damage

Scratches, scoring, out-of-round wear, and unstable operation may occur.

Brush material is too hard, contains abrasive particles, or has an unsuitable composition.

3

Excessive sparking and unstable operation

Risk of arcing. Current spikes, voltage fluctuations, and overheating may occur. Motor operation may become noisy and unstable.

Incorrect brush composition, poor contact, or mismatch with the operating conditions.

4

Increased contact resistance

Voltage drop and efficiency loss may occur.

Poor seating, contaminated contact surface, or insufficient conformity of the brush to the contact surface.

5

Breakdown of the contact film

An unstable or improper film may form on the commutator. The brush may operate with insufficient lubrication, causing sparking and micro-damage.

Brush material structure and composition do not match the operating speed or temperature conditions.

6

Damage to brush-holder springs or guides

Brushes may tilt, jam, or move poorly in the holder. Contact pressure may become unstable, causing sparking and vibration.

Incorrect brush dimensions, weight, stiffness, or design.

7

Emergency equipment failure

Sparking, overheating, or failure of the contact assembly may lead to motor or generator failure, including short circuits and winding damage.

Severe mismatch between the brush and the operating conditions, excessive sparking, overheating, or mechanical failure of the contact assembly.

5. Diagnosing a Brush Assembly During Improper Operation

No.

Symptom

What to Check

Possible Cause

1

Sparking at the commutator

Visual inspection during operation.

Incorrect brush composition or improper brush pressure from the brush-holder spring.

2

Excessive brush wear

Replacement frequency and remaining brush thickness.

Brush material is too soft, overheating, or high electrical resistance.

3

Commutator damage, scratches, or darkening

Inspect with the equipment switched off.

Brush is too hard, abrasive wear, or arcing.

4

Brush assembly overheating

Housing temperature, odor, thermal imaging.

Excessive resistance, poor contact, or sparking.

5

Uneven wear across the brush surface

Visual inspection and dimensional check.

Misaligned spring or brush holder, vibration.

6

Broken brush or chipped edges

Visual inspection and check for fragments inside the brush holder.

Brittle material, excessive vibration, or incorrect contact pressure.

7

Carbon dust contamination on the commutator

Clean and inspect the contact surface.

Excessive wear of the commutator bars.

8

Current fluctuations during operation

Ammeter readings or waveform analysis.

Uneven contact, poor seating, or brush material unsuitable for the operating conditions.

9

Unstable motor operation

Speed, noise, and vibration.

Combination of factors involving brush selection, mechanical condition, or current supply.

10

Rapid brush failure after replacement

Compare with the previous brush grade and review operating conditions.

Incorrect brush type, grade, or hardness.

6. Most Common Mistakes When Replacing Carbon Brushes

One of the main challenges for users is finding a brush with the correct design and dimensions. Installing a brush that is only close in size to the original is unacceptable (see tables). Excessive clearance between the brush and the brush holder can damage the brush holder itself.

Brush design is just as important to proper motor operation as the electrographite material from which the brush is made (see tables).

The most common mistakes when replacing brushes, based on many years of practical experience, include:

No.

Mistake / Misconception

Consequence

1

Installing a new brush without servicing and inspecting the commutator for surface smoothness, out-of-round condition, grooves, or microdefects.

Accelerated brush wear and reduced motor efficiency.

2

Replacing an imported brush with a textolite insulating plate with a domestically manufactured brush fitted with a metal plate (NK-1; NK-2).

Overheating and failure of the brush-holder spring.

3

Replacing a brush with tinned copper leads (PShML) with a brush using standard copper leads (PSh) in aggressive environments.

Oxidation of the copper leads, increased brush resistance, and overheating of the brush assembly.

4

Replacing an electrographite brush with a copper-graphite brush of similar design and dimensions, or vice versa.

Electrographite and copper-graphite brushes are not interchangeable.

5

Replacing a brush with “the same type that was previously installed” without checking the physical and technical parameters of the equipment.

A previous selection error may be repeated. Some imported motors may already have been supplied with incorrectly selected brushes.

6

Assuming that “any copper-graphite brush” can be used in current-collection assemblies of conductor rail systems.

A copper-graphite brush with the maximum copper content (MGSO grade) is required. Other copper-graphite grades may cause pitting of the copper conductor surface.

 
 

As can be seen from the above, a carbon brush is not simply a consumable component. It is a critical element that helps ensure the reliable and safe operation of electrical machines. When access to imported components is limited, brush selection should be based on the physical and technical parameters of the equipment specified in its technical documentation.

Successful replacement of imported carbon brushes with domestically manufactured alternatives depends both on material quality and on a professional approach to the diagnosis, maintenance, and operation of the current-collection assembly.

Recommendation: when selecting carbon brushes, especially for imported equipment, consult the brush manufacturer or a specialized service provider and provide accurate information on the operating conditions, machine type, and technical parameters.